Compression Strength

Compression Strength

Geo Technologies

Results of compression strength testing performed on concrete cylinders treated with Seal-It Concrete Sealant. These test results were submitted to us from a U.S. reseller.

The tests were performed only 7 days after the slurry mix was placed in the cylinder forms. Even though the concrete cylinders had not been given 28 days to cure, and the application method used was not recommended by Seal-It, there is an average increase in compression strength of 14.4% over the control cylinder.

Seal-It Concrete is a very user friendly product, and we believe you can achieve even better results. Seal-It personnel will help you with a custom application procedure for your project.