Waste Water, Bacteria and Concrete
Concrete and Bacteria:
A corrosive relationship.
Bacteria exist in our environment that are responsible for the breakdown of concrete. In short, a by-product of the living bacteria is sulphuric acid. Sulphuric acid and concrete are not a good mix.
The cost of this destructive mix was known only too well by a customer that contacted our St. Louis representative, SealMaxx of St. Louis . The customer, a concrete pipe manufacturer, was presently using a plastic liner to prevent corrosion caused by bacteria. Mr. Braden Schrum of Beco Concrete in St. Louis was searching for a more cost effective solution. Mr. Schrum liked what he saw that SealMaxx of St. Louis could do with Seal-It Concrete Sealant but needed to know specifically how this product would handle the destructive bacteria. This question led to the following, independent laboratory, findings.
BioBelt Laboratories of St. Peters, Missouri were contracted to determine what effect, if any, bacteria would have on concrete treated with Seal-It Concrete Sealant.
Two concrete cylinders that had been treated with Seal-It Concrete Sealant have microorganisms applied to them. Live bacteria were placed on 1 concrete cylinder; live fungi were placed on the second concrete cylinder. A third concrete cylinder was not treated with Seal-It Concrete Sealant and no microorganisms were placed on this cylinder.
Following progressively longer periods of time, each of the three concrete cylinders was “swabbed” as a method to collect any live organisms. These swabs were then placed in an environment where, if any were present, the organisms would multiply, and subsequently be detected.
As can be seen in the attached report from BioBelt Labs, no bacteria are present after any length of time, from 4 hours to 7 days, on the concrete cylinder which had been treated to the Seal-It Concrete Sealant.